Segment screw and barrel


Technical Parameter:

Hardness of  tempering HB260-320
Nitriding hardness HV950-1000
 Nitriding depth 0.5-0.8mm 
 Alloy hardness HRC58-65
Alloy depth 2.5-3mm
Nitriding brittleness  ≤ grade 1
Surface roughness Ra0.4 
 Straightness 0.015mm

 

ㅤWhy Choose Us?


ㅤRelated Products

_b_积木式平行双螺杆和机筒_ b_ (1).jpg

Segment extruder screw and barrel-

Segment extruder screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

积木式平行双螺杆和机筒.jpg

Segment PP granular screw and barrel-

Segment PP granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

橡胶机螺杆机筒 (4).jpg

Segment PE granular screw and barrel-

Segment PE granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

平行双螺杆机筒 (6).jpg

Segment PVC granular screw and barrel-

Segment PVC granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

积木式平行双螺杆和机筒 (1).jpg

Segment granular screw and barrel-

Segment granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

_b_积木式平行双螺杆和机筒_ b_.jpg

Segment screw and barrel-

Segment screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

_b_积木式平行双螺杆和机筒_ b_ (1).jpg

Segment extruder screw and barrel-

Segment extruder screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

积木式平行双螺杆和机筒.jpg

Segment PP granular screw and barrel-

Segment PP granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

橡胶机螺杆机筒 (4).jpg

Segment PE granular screw and barrel-

Segment PE granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

平行双螺杆机筒 (6).jpg

Segment PVC granular screw and barrel-

Segment PVC granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

积木式平行双螺杆和机筒 (1).jpg

Segment granular screw and barrel-

Segment granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

_b_积木式平行双螺杆和机筒_ b_.jpg

Segment screw and barrel-

Segment screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

_b_积木式平行双螺杆和机筒_ b_ (1).jpg

Segment extruder screw and barrel-

Segment extruder screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

积木式平行双螺杆和机筒.jpg

Segment PP granular screw and barrel-

Segment PP granular screw and barrel

Product Introduction: Material: 38CrMoAl、42CrMo、SKD-61 Useful: sapre parts for plastic extruder machine Application: Production plastic products Machinery Test Report: Provided Warranty time: 1 Year Export area: India, Viet Nam, TaiWai, HongKong, Ind...

ㅤSend Inquiry

Please Feel free to give your inquiry in the form below. We will reply you in 24 hours.
* Name
* Email
Phone
  • Angola+244
  • Afghanistan+93
  • Albania+355
  • Algeria+213
  • Andorra+376
  • Anguilla+1264
  • Antigua and Barbuda+1268
  • Argentina+54
  • Armenia+374
  • Ascension+247
  • Australia+61
  • Austria+43
  • Azerbaijan+994
  • Bahamas+1242
  • Bahrain+973
  • Bangladesh+880
  • Barbados+1246
  • Belarus+375
  • Belgium+32
  • Belize+501
  • Benin+229
  • Bermuda Is.+1441
  • Bolivia+591
  • Botswana+267
  • Brazil+55
  • Brunei+673
  • Bulgaria+359
  • Burkina+faso+226
  • Burma+95
  • Burundi+257
  • Cameroon+237
  • Canada+1
  • Cayman Is.+1345
  • Central African Republic+236
  • Chad+235
  • Chile+56
  • China+86
  • Colombia+57
  • Congo+242
  • Cook Is.+682
  • Costa Rica+506
  • Cuba+53
  • Cyprus+357
  • Czech Republic+420
  • Denmark+45
  • Djibouti+253
  • Dominica Rep.+1890
  • Ecuador+593
  • Egypt+20
  • EI Salvador+503
  • Estonia+372
  • Ethiopia+251
  • Fiji+679
  • Finland+358
  • France+33
  • French Guiana+594
  • Gabon+241
  • Gambia+220
  • Georgia+995
  • Germany+49
  • Ghana+233
  • Gibraltar+350
  • Greece+30
  • Grenada+1809
  • Guam+1671
  • Guatemala+502
  • Guinea+224
  • Guyana+592
  • Haiti+509
  • Honduras+504
  • Hongkong+852
  • Hungary+36
  • Iceland+354
  • India+91
  • Indonesia+62
  • Iran+98
  • Iraq+964
  • Ireland+353
  • Israel+972
  • Italy+39
  • Ivory Coast+225
  • Jamaica+1876
  • Japan+81
  • Jordan+962
  • Kampuchea (Cambodia )+855
  • Kazakstan+327
  • Kenya+254
  • Korea+82
  • Kuwait+965
  • Kyrgyzstan+331
  • Laos+856
  • Latvia+371
  • Lebanon+961
  • Lesotho+266
  • Liberia+231
  • Libya+218
  • Liechtenstein+423
  • Lithuania+370
  • Luxembourg+352
  • Macao+853
  • Madagascar+261
  • Malawi+265
  • Malaysia+60
  • Maldives+960
  • Mali+223
  • Malta+356
  • Mariana Is+1670
  • Martinique+596
  • Mauritius+230
  • Mexico+52
  • Moldova, Republic of+373
  • Monaco+377
  • Mongolia+976
  • Montserrat Is+1664
  • Morocco+212
  • Mozambique+258
  • Namibia+264
  • Nauru+674
  • Nepal+977
  • Netheriands Antilles+599
  • Netherlands+31
  • New Zealand+64
  • Nicaragua+505
  • Niger+227
  • Nigeria+234
  • North Korea+850
  • Norway+47
  • Oman+968
  • Pakistan+92
  • Panama+507
  • Papua New Cuinea+675
  • Paraguay+595
  • Peru+51
  • Philippines+63
  • Poland+48
  • French Polynesia+689
  • Portugal+351
  • Puerto Rico+1787
  • Qatar+974
  • Reunion+262
  • Romania+40
  • Russia+7
  • Saint Lueia+1758
  • Saint Vincent+1784
  • Samoa Eastern+684
  • Samoa Western+685
  • San Marino+378
  • Sao Tome and Principe+239
  • Saudi Arabia+966
  • Senegal+221
  • Seychelles+248
  • Sierra Leone+232
  • Singapore+65
  • Slovakia+421
  • Slovenia+386
  • Solomon Is+677
  • Somali+252
  • South Africa+27
  • Spain+34
  • Sri Lanka+94
  • St.Lucia+1758
  • St.Vincent+1784
  • Sudan+249
  • Suriname+597
  • Swaziland+268
  • Sweden+46
  • Switzerland+41
  • Syria+963
  • Taiwan+886
  • Tajikstan+992
  • Tanzania+255
  • Thailand+66
  • Togo+228
  • Tonga+676
  • Trinidad and Tobago+1809
  • Tunisia+216
  • Turkey+90
  • Turkmenistan+993
  • Uganda+256
  • Ukraine+380
  • United Arab Emirates+971
  • United Kiongdom+44
  • United States of America+1
  • Uruguay+598
  • Uzbekistan+233
  • Venezuela+58
  • Vietnam+84
  • Yemen+967
  • Yugoslavia+381
  • Zimbabwe+263
  • Zaire+243
  • Zambia+260
Country
* Message